The test is conducted at a certain temperature and humidity.The measurement method for crease recovery is to pass through90°Bent cardboard reply15After seconds, measure its recovery force. The measurement of cardboard stiffness is to
Application:
paper,Paperboard, paper box, ink coating industry
Wrinkle stiffness cuttercharacteristic:
Dual use: cardboard stiffness, crease stiffness
Measurement range:0~1000gf
digital display
Cardboard stiffness bending angle15°, crease stiffness, bending angle90°
Sample size of cardboard stiffness:70×
Accuracy:0.5 gf(Old model)C0039do1 gf)
Testing time:15S
Calibration weights:
Data interface:RS232
Standard:
BS 6965,BS 3748 ISO2493:1992(Old model)C0039Only meets the first two criteria)
power supply:220/ 240V@50HZ 110 V@60HZ (Please specify when placing an order)
External dimensions:H
weight: